GET A QUOTE
Stainless Steel Welding Wire GJ-ER310
GJ-ER310

Stainless Steel Welding Wire GJ-ER310

Copper-Free Solid Wire
(25Cr-20Ni fully austenitic, high-temperature)

  • AWS A5.9 ER310
  • EN ISO 14343-A-G 25 20

Product description

GJ-ER310 is a 25% chromium - 20% nickel fully austenitic stainless steel solid wire strictly complying with AWS A5.9 ER310. The high alloy content provides excellent oxidation resistance up to 1100C and is designed for welding 310 stainless and for high-temperature service applications.

Key Advantages

  • 01GUJIN

    Exceptional Oxidation Resistance: 25Cr-20Ni composition provides excellent resistance to oxidation and scaling at temperatures up to 1100C.

  • 02GUJIN

    Fully Austenitic: Zero ferrite weld metal offers maximum high-temperature ductility and creep resistance for severe thermal cycling.

  • 03GUJIN

    Thermal Fatigue Resistance: High nickel content provides excellent resistance to thermal fatigue in cyclic high-temperature service.

Application Guide

  • With Ar+2%O2 shielding: For welding 310/310S stainless in furnace components, heat treatment fixtures, and petrochemical heater tubes.

  • With 100% Ar (TIG): For welding heat-resistant cast alloys, radiant tubes, and high-temperature piping in power and process industries.

  • For dissimilar joints: Suitable for welding 310 to 304/316 and for buffer layers on creep-resistant steels in elevated temperature service.

Main constituents

Elements

C
(Carbon)

Si
(Silicon)

Mn
(Manganese)

Cr
(Chromium)

Ni
(Nickel)

Mo
(Molybdenum)

S
(Sulfur)

P (Phosphorus)

AWS Requirement

0.08 - 0.15

0.30 - 0.65

1.0 - 2.5

25.0 - 28.0

20.0 - 22.5

<=0.75

<=0.030

<=0.030

Typical Actual Value

0.11

0.45

1.70

26.0

21.0

0.20

0.008

0.015

Typical Mechanical Properties of Deposited Metal

Mechanical properties tested as all-weld metal with Ar+2%O2 shielding gas (DC+). AWS A5.9 does not specify minimum mechanical properties for austenitic stainless wires; values shown are industry typical results.

 

Test Item

Yield Strength

Tensile Strength

Elongation

Ferrite Number

AWS A5.9 Requirement

--

--

--

0 FN

Typical Actual Result

420 MPa

620 MPa

30%

0 FN

Reference Welding Parameters

Wire Diameter

0.8 mm (0.030")

1.0 mm (0.040")

1.2 mm (0.045")

1.6 mm (1/16")

Amperage

60 - 150

80 - 200

100 - 280

140 - 350

Voltage

18 - 22

20 - 26

22 - 30

24 - 34

WHY US

Consistent Quality, Direct Factory Pricing.

  • TECHNOLOGY
    GUJIN

    TECHNOLOGY

    100% batch consistency ensured by our advanced in-house QA lab.

  • EXPERIENCE
    GUJIN
    20
    +

    EXPERIENCE

    20+ years mastering SAW metallurgical synergy for heavy industries.

  • OEM SERVICE
    GUJIN

    OEM SERVICE

    Full OEM empowerment, from custom formulations to private labeling.

  • MANUFACTURING SCALE
    GUJIN

    MANUFACTURING SCALE

    Massive automated capacity to stabilize your bulk supply chain.

  • GLOBAL TRUST
    GUJIN

    GLOBAL TRUST

    Long-term partner to hundreds of industrial conglomerates worldwide.

FAQ

How do you prevent the agglomerated flux from absorbing moisture during long-distance sea freight?

Moisture control is critical for submerged‑arc welding fluxes. Our standard packaging is 25‑kilogram multi‑layer kraft paper bags lined with heavy‑duty moisture‑proof plastic bags. For extreme environments or ultra‑low hydrogen requirements (such as H5 grade), we can also provide custom heavy‑duty aluminium foil vacuum packaging. All goods are stacked on wooden pallets and tightly wrapped with multiple layers of industrial shrink film to ensure 100% dryness upon arrival at the port.

We are fabricating API 5L X70 pipes. Can we use standard neutral fluxes like GJ-301?

No. For High-Grade Oil & Gas pipeline fabrication (such as API X60 to X70), standard neutral fluxes like 301 or active fluxes like 501 are not suitable, as they cannot guarantee the required extreme low-temperature impact toughness. You must use our dedicated pipeline-grade Fluoride-Basic agglomerated flux, GJ-101Q (or GJ-101G), combined with Mo/Ni-alloyed wires (e.g., EA2 or S3Ni1Mo).This combination ensures zero loss of alloying elements and guarantees impact values of ≥27J(or much higher) at -40°C to -50°C.

What is your minimum order quantity (MOQ) and typical delivery time for a 20ft container?

Our standard MOQ for international orders is normally 5 tons per item. For a full 20‑foot FCL container, the loading capacity is usually 24 tons subject to container space constraints, and it can reach 27 tons without pallets. A 40HQ high‑cube container can hold a maximum of 28 tons. Backed by our robust production capacity, we can finish production, quality inspection and packaging within 7‑10 days upon receiving the deposit, and deliver the goods to major Chinese ports such as Qingdao Port or Tianjin Port.

Our workshop wants to save time and energy. Is there a way to use the agglomerated flux directly without the re-baking process?

Yes! We fully understand that re-baking costs time and electricity. For customers who want to skip this step, we highly recommend selecting our Heavy-Duty Aluminum Foil Vacuum Packaging. The flux is vacuum-sealed immediately after high-temperature manufacturing. When you open the bag in your workshop, the flux is in a 100% factory-dry state and can be poured directly into the welding hopper for immediate use.

Our steel plates have light rust and mill scale, and we cannot perfectly sandblast all of them before welding. Which flux can prevent porosity in this situation?

For structural steel with surface impurities like rust, oil, or mill scale, standard neutral or high-basic fluxes will likely cause porosity. You need our GJ-501A (Aluminate-Rutile Active Flux). It features a highly active deoxidizing slag system that offers exceptional tolerance to surface contaminants. This allows you to achieve flawless, X-ray quality welds at high speeds without rigorous pre-weld grinding, significantly boosting your shop floor efficiency.