Fused Flux
1.1
10-40mesh
25 kg plastic valve bags, 500/1000 kg large bags
When applied with welding wire such as H08A, H08MnA, H10Mn2 or H10MnSi, HJ431 can weld low carbon steel and some low alloy steel like 16Mn and 15MnV, as well as ships, boilers and low pressure vessels.
It can also be used for electroslag welding and copper welding.
Stable arc: It can maintain a very stable arc whether under DC or AC power supply, especially suitable for AC power.
Excellent slag detachability: After the weld cools, the slag will automatically curl up and can be removed with a light tap, which greatly improves the slag cleaning efficiency.
Beautiful weld formation: The weld surface is smooth and flat with fine and uniform lines.
| SiO₂ + TiO₂ | CaO + MgO | Al₂O₃ + MnO₂ | CaF₂ |
| 40–45 | 7–14 | 35–42 | 3–17 |
| Wire electrodes used | Yield strength ≥ MPa | Tensile strength ≥ MPa | Elongation8%≥% | Impactvalues≥J (CVN) | ||
| +20°C | -20°C | -40°C | ||||
| EL8 | ≥330 | ≥415 | ≥22 | 100 | 40 | — |
| EM12K | ≥390 | ≥415 | ≥22 | 110 | 50 | — |
| SU34 | 550 | 450 | 30 | — | 100 | — |
Drying temperature: 300°C–350°C
Holding time: 2 hours
Storage: After drying, it should be placed in an incubator at 100°C–150°C and taken as needed.
Exposure time: The exposure time in the air should not exceed 4 hours; otherwise, it needs to be dried again.
Strictly prohibited: Use flux that is damp, caked, or mixed with foreign objects.
Consistent Quality, Direct Factory Pricing.
100% batch consistency ensured by our advanced in-house QA lab.
20+ years mastering SAW metallurgical synergy for heavy industries.
Full OEM empowerment, from custom formulations to private labeling.
Massive automated capacity to stabilize your bulk supply chain.
Long-term partner to hundreds of industrial conglomerates worldwide.
Moisture control is critical for submerged‑arc welding fluxes. Our standard packaging is 25‑kilogram multi‑layer kraft paper bags lined with heavy‑duty moisture‑proof plastic bags. For extreme environments or ultra‑low hydrogen requirements (such as H5 grade), we can also provide custom heavy‑duty aluminium foil vacuum packaging. All goods are stacked on wooden pallets and tightly wrapped with multiple layers of industrial shrink film to ensure 100% dryness upon arrival at the port.
No. For High-Grade Oil & Gas pipeline fabrication (such as API X60 to X70), standard neutral fluxes like 301 or active fluxes like 501 are not suitable, as they cannot guarantee the required extreme low-temperature impact toughness. You must use our dedicated pipeline-grade Fluoride-Basic agglomerated flux, GJ-101Q (or GJ-101G), combined with Mo/Ni-alloyed wires (e.g., EA2 or S3Ni1Mo).This combination ensures zero loss of alloying elements and guarantees impact values of ≥27J(or much higher) at -40°C to -50°C.
Our standard MOQ for international orders is normally 5 tons per item. For a full 20‑foot FCL container, the loading capacity is usually 24 tons subject to container space constraints, and it can reach 27 tons without pallets. A 40HQ high‑cube container can hold a maximum of 28 tons. Backed by our robust production capacity, we can finish production, quality inspection and packaging within 7‑10 days upon receiving the deposit, and deliver the goods to major Chinese ports such as Qingdao Port or Tianjin Port.
Yes! We fully understand that re-baking costs time and electricity. For customers who want to skip this step, we highly recommend selecting our Heavy-Duty Aluminum Foil Vacuum Packaging. The flux is vacuum-sealed immediately after high-temperature manufacturing. When you open the bag in your workshop, the flux is in a 100% factory-dry state and can be poured directly into the welding hopper for immediate use.
For structural steel with surface impurities like rust, oil, or mill scale, standard neutral or high-basic fluxes will likely cause porosity. You need our GJ-501A (Aluminate-Rutile Active Flux). It features a highly active deoxidizing slag system that offers exceptional tolerance to surface contaminants. This allows you to achieve flawless, X-ray quality welds at high speeds without rigorous pre-weld grinding, significantly boosting your shop floor efficiency.